Hi guys. I received an interesting question today and I think I know the answer but I want to hear what you think.
For a P2.2/P2.3 material ASME B16.5 flange that is dual-marked as 316/316L, what would you use as the allowable stress at, say, 200° F? The problem is the two materials have different MAWP's. At 200 F, 316 has MAWP of 240 psig and 316L has MAWP of 195 psig.
I am not aware if the B31 Codes address this question.
What say ye? Thanks guys!
For a P2.2/P2.3 material ASME B16.5 flange that is dual-marked as 316/316L, what would you use as the allowable stress at, say, 200° F? The problem is the two materials have different MAWP's. At 200 F, 316 has MAWP of 240 psig and 316L has MAWP of 195 psig.
I am not aware if the B31 Codes address this question.
What say ye? Thanks guys!