Can anyone advise on water injection pipeline material that Petrobras and Statoil have used? I know, that depending on confidence and availability of topsides processing to reduce oxygen levels, some operators will use carbon steel. However, many operators have had failures and as such prefer to use liners or CRA pipelines. I am not familiar with Petrobras or Statoils water injection lines and wonder if anyone can help me. Thanks
 
Material for water injection pipelines is CS+6mm CA with corrosion inhibition.Based company recommendation we can go for CS with FBE lining also.
No need to go for CRA option.

 