Can anybody tell me what material the M16 stud from a car and any website that can give me the material tensile strength toughness and magnetic properties
 
Replies continue below

Recommended for you

The material and properties will depend upon the property class of the stud. Can you tell us about the application? Does it have any markings on it?

Here is a chart for mechanical property requirements for metric fasteners:


Here is a chart for chemical composition requirements:


I cannot help you with magnetic properties.

Regards,

Cory