I need to supply 34.92 mm dia En10025 grade S355J2G3.
Can i use 150M19 if so what treatment do i need to carry out to meet the properties UTS 510/680 n/mm2 Yield 345n/mm2 min
Elongation 15% min Impacts @-20 C KVJ 27min
 
Replies continue below

Recommended for you

Unless the S355J2G3 designation also includes +N, then the delivery condition is supposed to be as hot-rolled, meaning no additional thermal treatment.
 