Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations MintJulep on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

MATERIAL SPECIFICATION INDUSTRY STANDARD FOR "STOCK" MATERIAL TOLERANCES 3

Status
Not open for further replies.

DiegoLGraves

Mechanical
Joined
May 22, 2008
Messages
209
Location
US
We frequently see this note on a major customer's prints: REFER TO THE MATERIAL SPECIFICATION INDUSTRY STANDARD FOR "STOCK" MATERIAL TOLERANCES. This has usually been read here as referring to the material thickness rather than material properties. Looking at the ASTM B209 spec for the item I'm working on, and other ASTM material specs, I don't see any reference to thickness tolerances, only chemical and mechanical properties. Are there specifications for thicknesses? We purchase material per spec, mostly steel and aluminum sheet and plate, and bar stock.

Regards, Diego

 
An example of an ASTM Steel specification that discusses thickness and tolerance is: A513, titled: Standard Specification for Electric-Resistance-Welded
Carbon and Alloy Steel Mechanical Tubing.

This specification covers chemistry, dimensional, and surface specification.


Nick
 
For bars check out ASTM A108. It should contain size tolerances.
 
For Aluminum Mill products you can use ANSI H35.2 American National Standard Dimensional Tolerances for Aluminum Mill Products

This is called out in the B209 specification at section 2.3

It covers just about all shapes and forms.

 
Thanks to each of you for your help, it is appreciated. I needed to do a closer reading of the specs before asking here.

Kind regards, Diego
 
Just in case - for sheet metal try SAE J1058.

Although technically it's limited to vehicles.
 