Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations MintJulep on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Material selection for 2" piggyback pieline carrying Corrosion inhibit

Status
Not open for further replies.

sayee1

Materials
Joined
Feb 6, 2003
Messages
281
Location
SA
Need advice on selection of material for the following 2" piggy back pileine carrying corrosion inhibitor as per details below:
Chemical Composition:
Aromatic Naptha: 50 – 70% (w/w)
Composition Comments: A proprietary blend of amine derivatives and fatty acids in an aromatic solvent.

Physical Properties:
Appreance: Clear liquid Amber coloured
Specific Gravity @25deg: 0.924
Pour Point: Less than 0 deg C
Viscosity @25deg: 40-50 cps
Flash point (PMCC): more than 65 deg C
Solubility: Soluble in Aromatic hydrocarbon.


Thanks and regards
Sayee Prasad R
Ph: 0097143968906
Mob: 00971507682668
email: sayee_prasad@yahoo.com
If it moves, train it...if it doesn't move, calibrate it...if it isn't written down, it never happened!
 
If the fluid is sold in the US I think it is required to have an MSDS (Material Safety Data Sheet) available from the manufacturer. The MSDS usually (always?) includes statements about any corrosive properties. The manufacturer should be able to provide material recommendations for piping, although I suspect that mild steel would be OK in this case.
 
Status