I have an environment Low pressure , low temperature reservoir with the following concentration:

H2S : >1000 ppm
CO2 : >200 ppm

Can you please advise on material selection.

tnx
 
The advice is to obtain a more detailed listing of environmental parameters and consult a qualified materials & corrosion engineer. You could probably look at NORSOK M-001 to begin with,


in order to get an idea of options. This forum will not give you any sensible selections with that sparse data, as well as having to get involved with ISO 15156.

Steve Jones
Materials & Corrosion Engineer


All answers are personal opinions only and are in no way connected with any employer.
 
Tnx Steve for your direction
 