good morning
i aa asking if anyone can give me comparison between materials
S 355 J0 EN 10025 and ASTM SA 516 GR.70 for a water storage tank thanks and im available for any information's can help .
thanks in advance.
 
There is an equivalent of S 355 JR which is ASTM A 572 Gr 50. Pls look to the page 48 of the attached doc.
If you can provide more info.( design temperature, applicable standards, available material, size of the tank ..) you may get better responds.
 