Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations cowski on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Material properties 3

Status
Not open for further replies.

wgr4895

Mechanical
Apr 23, 2002
5
Hi,
Could anyone fowarder me a material properties like ultimate strength,yield strength, thermal coefficient etc for this material :
1. "COrten steel"
2. Rockwool
Thanks
 
Replies continue below

Recommended for you

COR-TEN is a tradename used by U.S. Steel for a group of HSLA structural steels. You can find information on these grades, including mechanical properties, at the following website:


The coefficient of thermal expansion depends on temperature, and to some extent on alloying content. The following data is for a C-Mn-Si steel, which is what COR-TEN is:

CTE Temperature
(in micrometers/m C) (in degrees C)

9.5 25
11.5 100
13.5 200
15.0 300
16.0 400
16.4 500
16.6 600

Note that this data is not averaged. IF you want an averaged number, then something like the following values would be more appropriate

AVG CTE
10.2 from 20-100 C
13.5 from 20-400 C
14.4 from 20-600 C

As for Rockwool, I am not familiar with this name. You may try the following website for info:

 
Rockwool is a trade name for a type of mineral fibre insulation made by, would you believe, Rockwool. Their main site is very comprehensive and should contain most of the info you are looking for.