Does ETABS has automatic properties for C30, C35, C40 concrete? I am having a hard time filling the material properties dialog box in etabs if I want to change to,ie, C35. Is there any reference that I can look up to in knowing different properties(I've tried to search on the internet but it doesnt relate to ETABS dialog box for properties).
 
No, you will have to define this manually. I have copy pasted the information for you from the ETABS model.
Units are KN,mm

MATERIAL "CM20" M 2.402E-12 W 2.356E-08 TYPE "ISOTROPIC" E 22.36 U 0.2 A 9.89999989542412E-06
MATERIAL "CM20" DESIGNTYPE "CONCRETE" FY 0.5 FC 0.02 FYS 0.5
MATERIAL "CM25" M 2.402E-12 W 2.356E-08 TYPE "ISOTROPIC" E 25 U 0.2 A 9.89999989542412E-06
MATERIAL "CM25" DESIGNTYPE "CONCRETE" FY 0.5 FC 0.025 FYS 0.5
MATERIAL "CM30" M 2.402E-12 W 2.356E-08 TYPE "ISOTROPIC" E 27.386 U 0.2 A 9.89999989542412E-06
MATERIAL "CM30" DESIGNTYPE "CONCRETE" FY 0.5 FC 0.03 FYS 0.5
MATERIAL "CM35" M 2.402E-12 W 2.356E-08 TYPE "ISOTROPIC" E 29.58 U 0.2 A 9.89999989542412E-06
MATERIAL "CM35" DESIGNTYPE "CONCRETE" FY 0.5 FC 0.035 FYS 0.5
MATERIAL "CM40" M 2.402E-12 W 2.356E-08 TYPE "ISOTROPIC" E 31.623 U 0.2 A 9.89999989542412E-06
MATERIAL "CM40" DESIGNTYPE "CONCRETE" FY 0.5 FC 0.04 FYS 0.5
MATERIAL "CM45" M 2.402E-12 W 2.356E-08 TYPE "ISOTROPIC" E 33.541 U 0.2 A 9.89999989542412E-06
MATERIAL "CM45" DESIGNTYPE "CONCRETE" FY 0.5 FC 0.045 FYS 0.5
MATERIAL "CM50" M 2.402E-12 W 2.356E-08 TYPE "ISOTROPIC" E 35.355 U 0.2 A 9.89999989542412E-06
MATERIAL "CM50" DESIGNTYPE "CONCRETE" FY 0.5 FC 0.05 FYS 0.5
MATERIAL "CM60" M 2.402E-12 W 2.356E-08 TYPE "ISOTROPIC" E 38.729 U 0.2 A 9.89999989542412E-06
MATERIAL "CM60" DESIGNTYPE "CONCRETE" FY 0.5 FC 0.06 FYS 0.5

 