What mechanical properties beyond those on the Allegheny Ludlum page above?
Perhaps mechanical properties are not so readily dictated by the electromagnetic ones -- ASTM A867 gives typical Rockwell hardnesses from 60 to 100 HRB, plus HRC 23. Thermal & mechanical history (annealing vs. cold work) and Si content appear to be direct factors. None of the ASTM electrical steel specs. that I looked at give mechanical properties, although some could be computed from ductility & hardness data.