Hi All,
I need material properties, primarily tensile strength, on 20 mil thick pvc film used for boat and tent windows, seat covers etc. This material is described as double polished, optically clear and cold crack resistant to -40 F
Can anybody help with tensile strength details?
Thanks
JQCF1
I need material properties, primarily tensile strength, on 20 mil thick pvc film used for boat and tent windows, seat covers etc. This material is described as double polished, optically clear and cold crack resistant to -40 F
Can anybody help with tensile strength details?
Thanks
JQCF1