Dec 16, 2002 #1 alikaynak Mechanical Joined Dec 16, 2002 Messages 1 Location TR I want to learn that which one is the best choice CuSn5ZnPb5 (bronze) or Navy Brass (Cu62%-Zn 36.2%-PB 1.75%-AS 0.06%)to use for gate valve thrust collar made by?