Applying for CRN category "C". They are not flange valves. I need help, material of the body is St St 305 ASTM A-240. it is listed material but Code listed allowable stress for 100F temp only and product is designed for 150F. I checked ASME SecII D, material is listed there SA-240, 305 AND Su is listed in U table and yield is in Y-1 table.
Values are different B31.3
Tensile = 70ksi
yield = 25ksi
Allowable Stress = 16.7 ksi @ 100F
While
Values in ASME Sec II D
Tensile = 75@ 100F and 71.1 at 150F (Table U)
Yield = 30@ 100f and 26.7 @ 200F
Is there provision in B31.3 that data from AMSE SEC II D can be extrapolated for elevated temp and used in the calculation.
Regards,
Values are different B31.3
Tensile = 70ksi
yield = 25ksi
Allowable Stress = 16.7 ksi @ 100F
While
Values in ASME Sec II D
Tensile = 75@ 100F and 71.1 at 150F (Table U)
Yield = 30@ 100f and 26.7 @ 200F
Is there provision in B31.3 that data from AMSE SEC II D can be extrapolated for elevated temp and used in the calculation.
Regards,