Hello:

It seems for me that it does not include 5 Gr-1/2 mo ( P5B- Gr 1 ) group material into Table UHA-32. Does it mean that 5 Gr- 1/2 mo group material not consider as high alloy materail , so the requirement as per UHA does not apply for it. Please clarify .

Thanks

Abraham Hong
 
Replies continue below

Recommended for you

Please look at Part UCS of ASME Section VIII, Div 1. This material is not high alloy, it falls under UCS, Table UCS-56.
 