Material for burner nozzle

Status
Not open for further replies.

arunmrao

Materials
Oct 1, 2000
4,758
I am seeking an alternate material for a coal burner nozzle used in a cement kiln. Currently 310 grade stainless steel is used. However due to the abrasive conditions the wear out is rapid. Iam thinking of substituting by a tool steel material. Any help or suggestion welcome.
 
Replies continue below

Recommended for you

I have experience in replacing high temperature metal nozzles with plastic materials. They offer superior wear to say stainless, but the temperaure limitations are around
500 degrees F. I would suggest a bearing grade of Ryton, PEEK or Polyimide all have
tensile's of 15,000 to 35,000 psi.

You may check out <
Good Luck
 
You didn't indicate what your operating temperature is. If it is below 1000 F, have you considered a carbidic grey iron? Chromium alloyed gray iron can develop considerable carbide content (10-25%) which has excellent wear resistance. CWC produces a material they call proferal or super proferal that is used for engine camshafts. I would think such a material would provide substantial improvement over 310 stainless.
 
The better materials for nozzles at high temp. and abrasion are made with silicium carbide, silicium nitride or mix of the two.Ask to makers of ceramic kilns.
 