MATERIAL F-1.2379

Status
Not open for further replies.

SVanden

Mechanical
Feb 25, 2003
17
We have had tooling designed and fabricated in Spain, and the material is called out as F-1.2379 HRc 60-62. Is this D2??

Thanks
Svanden
 
Replies continue below

Recommended for you

Yes that is D2 tool steel....
nick

Nick