Seems like this should be in all the tubing catalogs, but I can't find it. I am looking for a material compatability table for Polyurethane and Polyethylene tubing vs Ozone and/or Propylene Glycol. Does anyone have a good source or web link?



Thanks
Bill
 
This table has chemical resistance for many polymers. As Pat said, when you need detailed information for a certain polymer, you'll need to contact the manufacturer or check their website.


Chris DeArmitt

"Knowledge has no value except that which can be gained from its application toward some worthwhile end."
Think and Grow Rich - Napoleon Hill
 
The MAT WEB site was of no help. I don't know the exact compounds that are being used to make the tubing. It lists typical properties but not compatabilites? Unless I missed it.
I could call the manufacturer ( Parker), I tried their website, but didn't find anything on compatability.

Thanks
Bill
 
I still don't have a direction. Polyethylene and Polyurethane tubing both have similar compatibilites to Propolene Glycol, depending on which website you go to. Some sites rate them equal, others rate PE better than PU. I believe Polyethylene to be the more compatable choice?


Thanks
Bill
 
There are several types of PU which have quite different chemical resistance properties. Polyester and polyether types spring to mind, but there are significant variations within each type and I think also some other types.


Bayer, BASF, Merquinsa, Dow and Noveon are major suppliers and should cover most types between them

Regards
Pat
See FAQ731-376 for tips on use of eng-tips by professional engineers &
for site rules
 
Laboratory equipment suppliers (like Nalgene or Plamer Labs.) sometimes have compatibility charts in their technical literature.
 