Hi everbody
May you please give me a figure of erosion velocity in marine hose? As you know, erosion velocity in carbon steel marine pipeline is about 5-6 m/s. But, as i see in marine projects, marine hoses with internal linining, are choosed by a smaller diameter. Is it correct that they can beer more velocities?
Thanks
 
Replies continue below

Recommended for you

OCIMF guidline for marine hoses recommend 14m/s. I have confirmed this value with Bridgestone representative in my area.
Regards
 