Making A Soft Plastic Tray 1

Status
Not open for further replies.

vcand

Military
Apr 20, 2006
1
Hello All,

I am currently interested in trying to find a way that I can make a plastic tray at home. I'm sure everyone's seen one, they come in board game boxes and generally they hold the cards, pieces, dice, etc. I do not need mass production only like 1-2 (5 on the high side). I've read a lot of post where they're talking about doing solid plastic molding at home, which I guess is an option but it seems like a waste of materials and add's unneeded weight. It's don't think making the mold would be the problem (as I'm sure I could use clay, plaster, wood, stone, algenate, whatever to make a positive/negative), but I'm not sure where to get the plastic to do this type of thing.

Any ideas would be appreciated.
Thanks,
Vincent
 
Replies continue below

Recommended for you

Buy some PVC sheet from a local sheet plastics supplier.

Make a male mould from wood.

Set the oven to the temperature recommended by the sheet supplier. From memory, about 110 to 120 Deg C should do.

Heat the sheet in an oven until it is soft.

Drape the sheet over the mould and press it down by hand. Use a leather riggers glove to protect from heat.



Regards

eng-tips, by professional engineers for professional engineers
Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora.
 
Make a CAD model and have a few made on a Zcorp 3D printer. There are many such machines about which are underutilized. Some folks are looking for projects just to keep in practice.
 