Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations MintJulep on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

maintenance pvc roof

Status
Not open for further replies.

Cuyanausul

Mechanical
Joined
Aug 27, 2005
Messages
67
Location
SV
Hello, I am helping a company taht has a roof protected with a membrane that feels like pvc, be it or not, after 10 years it has become stiff and at some places is breaking ans the joints are going separated. Does any one have any recomendations on how to repair it?, I believe there are some products to return the membrane it`s flexibility and make it last longer. I read somewhere that UV rays make oils from some polymers go away???
Thanks in advance
 
PVC, both rigid & plasticized, gets destroyed by sunlight (UV). Gets brittle and cracks at very low stress (after a few years). Exposed PVC pipe (rigid) is commonly painted for protection. Much harder for paint to adhere to flexible vinyl, but can do after a solvent wipe.

As to repairs: I think the PVC polymer structure is damaged, so not much point adding plasticizer. Either replace the whole, or patch overlays as needed. The PVC cement sold for rigid PVC will not work for flexible vinyl, but I've bonded flexible vinyl using a special cement (tetrahydrofuran? containing dissolved PVC) from Flexi-Liner:
 
Thank you so much for your help, I believe we will recomend changing all the material, after 10 years it has reached it`s life expentancy.
 