What is the general consensus on MT on ferromagnetic steels, welded with an austenitic stainless filler?
Can this be done? If so, are there limitations on the acceptance criteria, is the accuracy as high as when performed on all magnetic joints?
I am by no means an NDT expert, I just had a quick browse through the (ISO) MT standards, and this case does not seem to be mentioned.
I know PT (dye penetrant testing) is an alternative, but I have High strength parts that were welded with a 309 filler, and MT has been performed (possible the MT operator was not aware of the filler metal that was used). I would like to know whether or not I can trust these test reports.
Thanks for your input.
Can this be done? If so, are there limitations on the acceptance criteria, is the accuracy as high as when performed on all magnetic joints?
I am by no means an NDT expert, I just had a quick browse through the (ISO) MT standards, and this case does not seem to be mentioned.
I know PT (dye penetrant testing) is an alternative, but I have High strength parts that were welded with a 309 filler, and MT has been performed (possible the MT operator was not aware of the filler metal that was used). I would like to know whether or not I can trust these test reports.