Does any one know the magnetic permeability of Cronite HR6 high temp stainless (made up of 0.4-C; 25-Cr; 20-Ni; 1-Mn; 1.1-Si) or any other material resembling the above. I know RA-330 is very similar...

Thanks in advance,
Alek Derejian
 