Magnetic field induced martensite 4

Status
Not open for further replies.

Greenleader

Aerospace
Joined
Aug 10, 2004
Messages
68
Location
US
I am not a metallurgist, so please be easy with the terms. I have a question; is magnetic field induced martensite, and strain induced martensite, different terms for the same process? Thanks, Gerald
 
Whoa!! Heavy stuff but I think they answer your question.
It appears that they are not the same, the magnetic field induced transformation seems to be a reversible phenomenon in some shape memory alloys and only exists while the field is applied.Stain induced transformation is however not reversible and can occur in more conventional alloys.
 
Much obliged, metenger!

I just discovered this topic, so I have a lot of reading to do. Thanks again, Jerry
 
As meteng pointed out, there can be a transformation from austenite to martensite induced by applying a magnetic field which reverses with the removal of the field. The strain induced transformation requires significant plastic deformation and remains after the stress which imposed the strain is removed.
 
I learnt something new. Though this was vaguely in my memory that one transformation is reversible while the other is not. Great posting and equally good responses.
 
Greenleader,

For more reading on the subject, the following link gives some practial applications of strain induced martensite:

forums/0001.htm



 