Oct 27, 2005 #1 AeroAd New member Joined Aug 12, 2005 Messages 8 Location CA Does someone know the hardness (Vickers, Brinell...) of the magnesium alloy AMS4439 or does someone know a good site or book to find tables of hardness for magnesium alloys. Thanks Adam
Does someone know the hardness (Vickers, Brinell...) of the magnesium alloy AMS4439 or does someone know a good site or book to find tables of hardness for magnesium alloys. Thanks Adam
Oct 27, 2005 #2 CoryPad Materials Joined Apr 15, 2002 Messages 5,192 Location US The ASM Handbook shows 62 HB. ASM sells a Magnesium handbook: http://www.asminternational.org/Tem...=Ecommerce/ProductDisplay.cfm&ProductID=10522 Regards, Cory Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora. Upvote 0 Downvote
The ASM Handbook shows 62 HB. ASM sells a Magnesium handbook: http://www.asminternational.org/Tem...=Ecommerce/ProductDisplay.cfm&ProductID=10522 Regards, Cory Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora.
Oct 27, 2005 #3 israelkk Aerospace Joined Dec 30, 2002 Messages 2,280 Location IL MIL-HDBK-5J which brings the data from the AMS onlyspecify tensile and compressive values. Hardness is not guaratied same as with PH steels. Upvote 0 Downvote
MIL-HDBK-5J which brings the data from the AMS onlyspecify tensile and compressive values. Hardness is not guaratied same as with PH steels.
Oct 27, 2005 #4 WKTaylor Well-known member Joined Sep 24, 2001 Messages 4,308 Location US Aeroad... MS4439E provides hardness test requirements... and defines what they mean. See AMS4439 Para 8.3... Regards, Wil Taylor Upvote 0 Downvote
Aeroad... MS4439E provides hardness test requirements... and defines what they mean. See AMS4439 Para 8.3... Regards, Wil Taylor