Mar 29, 2006 #1 me66us Aerospace Joined Mar 29, 2006 Messages 3 Location US We have parts about 1" OD tungsten we would like to machine on CNC turning. Any one has idea or recommendation how we can machine tungsten Thanks Advance
We have parts about 1" OD tungsten we would like to machine on CNC turning. Any one has idea or recommendation how we can machine tungsten Thanks Advance
Mar 29, 2006 #2 mrainey Industrial Joined Jun 22, 2002 Messages 225 Location US http://www.eng-tips.com/viewthread.cfm?qid=105708 Software For Metalworking http://mrainey.freeservers.com Upvote 0 Downvote
http://www.eng-tips.com/viewthread.cfm?qid=105708 Software For Metalworking http://mrainey.freeservers.com