Hercules28
Materials
Dear all,
Looking into information on machining Super duplex stainless steels.
Except carbide tools, is anybody using something more efficient?
They are getting confused very fast.
Some literature to read would also be appreciated.
Thanks,
Herc
Looking into information on machining Super duplex stainless steels.
Except carbide tools, is anybody using something more efficient?
They are getting confused very fast.
Some literature to read would also be appreciated.
Thanks,
Herc