Nov 7, 2007 #1 vscid Nuclear Joined Aug 5, 2007 Messages 65 Location US Hi, Whats the shield gas (Argon) typical pressure at which machine TIG welding is performed? Thnks! Vscid
Hi, Whats the shield gas (Argon) typical pressure at which machine TIG welding is performed? Thnks! Vscid
Nov 7, 2007 #2 metengr Materials Joined Oct 2, 2003 Messages 15,478 Location US More critical is the flow rate of Argon to properly shield the weld puddle. You need to optimize (establish) this flow rate based on your joint configuration. Upvote 0 Downvote
More critical is the flow rate of Argon to properly shield the weld puddle. You need to optimize (establish) this flow rate based on your joint configuration.