Lubricomp GFL-4034 EM M Polysulfone.
I need tensile modulus and CTE, but could find only Flexural Modulus on MatWeb.
Does anybody know these parameters vaue, please?
Thank you.
 
Replies continue below

Recommended for you

For low aspect ratio fillers like milled glass fiber you can assume that flexural modulus is close to the tensile modulus, i.e. 3.45 GPa 500 ksi.

Chris DeArmitt

"Knowledge has no value except that which can be gained from its application toward some worthwhile end."