We have started using it, in the SW US, but are having problems with longitudinal cracking along the wheel path. I'm thinking that maybe the lower temperature limit is not low enough, or the deviation from average low is not compensated for adequately. In any case it appears that the oil is too brittle. Anybody else using this?
 