Hi All,

I'm trying to track down material property information for LP-314-T2 sheet. It seems to come under a generic LN 9073 standard. I have to carry out a sheet metal repair to an aircraft with this type of skin, but can find any reference to LP-314-T2 anywhere and only basic references to LN9073. I was hoping to replace with 2024-T3 but have no idea what the mechanical properties are.

Any help appreciated.

Thanks,

 
The German Standard LN 93 is available from

LN 9073 - Complete Document
Revision: 91 Chg: Date: 09/00/91
AEROSPACE; SHEET AND PLATE IN WROUGHT ALUMINIUM ALLOYS, STANDARD PLANE, ROLLED; DIMENSIONS MASSES

Comments: GERMAN

It probably lists different materials

 