Is good the ASTM A36 structural steel for a low temperature sites (-58 degrees F) or what is the yield strenght under this temperature?
 
Replies continue below

Recommended for you

No, ASTM A36 is not suitable for -58 deg F. The yield strength would be close to 36 Ksi from room temperature and below.
 