Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations IRstuff on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Low Temperature, High Vacuum Bearings 1

Status
Not open for further replies.

Mark172

Aerospace
Aug 26, 2008
43
Hi All,

I'm having a hell of a time finding a supplier of low temp high vacuum bearings with lead times under 14 weeks. Does anyone know of a good supplier? Basic (flexible) requirements:

Temp: -100C to 50C
Vacuum: to 10^-7 Torr
Radial load: 100 lbf
Outgassing: NASA spaceflight requirements (<1% TML, <0.1% CVCM)

Any suggestions you have are greatly appreciated!!!
 
Replies continue below

Recommended for you

I apologize that I forgot one more key piece of information: these are small bearings, ~1" diam.
 
Is this for a mechanical feed-through into vacuum chamber?

If not would all ceramic ball bearings fit the bill? No lub. or plastic parts.
 
Mark172-

I did some mechanical systems design work on the Shuttle program and the typical radial ball bearing used for mechanisms located in the payload bay was 440C race/ball material. These were standard catalog instrument type bearings, except that we would solvent clean and re-lubricate them with a low-temp vacuum grease like Braycote 600EF. If we needed a shaft seal to keep the grease from migrating we would use PTFE Omniseals, provided the shaft surface speed was low.

A standard 440C instrument ball bearing with an OD under 1.0" should easily handle a 100lbf radial load. There are dozens of companies that offer such standard catalog ball bearings, so it should be no problem to obtain a small quantity in less than 14 weeks.

Hope that helps.
Terry
 
Terry, that's just the kind of information I was hoping for. Thanks so much! This gives me enough of a lead that I think I'll be able to find a good solution.