Low temp application for Incoloy 800 2

Status
Not open for further replies.

heaterguy

Mechanical
Nov 15, 2004
99
Will Incoloy 800 have any problem operating in -100 deg. F inside of a pressure vessel designed for -265 deg. F? The electric heater inside of a liquid blow down tank has an Incoloy 800 sheath.
 
Replies continue below

Recommended for you

Yes, the Incoloy 800 sheath material should be acceptable for use at this service temperature.
 