I am trying to compose a letter to an engineer requesting that they consider the use of "as-welded" stainless steel 316L pipe and fittings for low pressure air pipe lines utilized in a wastewater treatment plant, in lieu of seamless. The temperature is 280 deg F or less with a test pressure of 50 PSI. The lines are 12" NPS or less stainless steel. Any suggestions or points to make?
 
This application sounds like blower air for a biological reactor. Spiral wound stainless teel is routinely used for such applications in Sydney Water Corporation.

“The beautiful thing about learning is that no one can take it away from you.”
---B.B. King
 
No problem using SWSS or ERW up to much higher pressures for such service. You should however consider a duplex stainless as you may get stress corrosion cracking with the high chlorides seen in WWTPs. SAF 2205 would be a better choice than 316L. has some very good articles on such applications.