Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations MintJulep on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Low Chloride content gasket for Stailess steel girth flange

Status
Not open for further replies.

roniprabowo

Mechanical
Joined
Dec 22, 2003
Messages
22
Location
ID
Hai all,
Does anyone know why low chloride content gasket require for stainless steel girth flange ?
Is there any reaction between Cl and Stainless steel ?
Look forward for the information.
 
The Achilles heel of low-Mo aust. SS is Cl. Pitting and SCC are what happens.
 
To add to Metalguy's statement, stainless steels are highly susceptible to crevice corrosion due to chlorides - even the high molybdenum grades. It is highly advisable to eliminate chlorides from known crevices.

 