i am looking for aluminum epoxy so i can make some molds.

i am wondering if body filler would work.

if not where..... all i seem to get is people who want to make the mold for me......

also. what would be a good release agent for pe or pp with this mold......

thanks
 
There was a product called Devcon. I don't know if it's still available, but you could try to Google it

Regards
Pat
See FAQ731-376 for tips on use of eng-tips by professional engineers &
for site rules
 
Real aluminum makes a much better mold, and 'cures' faster.



Mike Halloran
Pembroke Pines, FL, USA
 
No shrinkage, right Mike? [bigcheeks]

Dan - Owner
Footwell%20Animation%20Tiny.gif
 
Not in the same league as epoxy.

Okay, ... I really get a kick out of putting chips on the ceiling.

;-)



Mike Halloran
Pembroke Pines, FL, USA
 
i am trying to get my milling machine up, bad brakes. i have to have the shoe relined.

anyway so what do you mean chips in the ceiling?

any ideas of where i can get the stuff or what it is called?

jim
 
After very little thought and almost no effort I managed to type devcon into google. To my astonishment this was the first hit. You should try it some time.


Regards
Pat
See FAQ731-376 for tips on use of eng-tips by professional engineers &
for site rules
 
Aluminum can be machined at pretty high speeds.

I especially like 2024, which makes a beautiful short chip if you're cutting it fast enough.

When you're cutting fast, and the chips are breaking correctly, a horizontal spindle will throw chips up far enough to hit a lot of shop ceilings.



Mike Halloran
Pembroke Pines, FL, USA
 
ok sorry to frustrate you pat, i did look at devcon website and didn't know what i was looking for sin they have have plethora of products.


thanks mcgyvr
thanks mike for the clarification
 
Look for an aluminium filled grade of epoxy with minimum shrinkage and good conductivity and recomended for moulds. I don't remember any more without doing the same search.