i am working for a european scientist who requires <br>
a grade of aluminum only found in europe. the material <br>
is anticorodal-100. the composition, i think, is AlMgSil. <br>
do you have a material with these specifications? i need <br>
two rounds, 6&quot; dia. x 1&quot; thick.<br>
i've been informed that this material is called 6063 here<br>
in the u.s. and it is an extruded material only. so now <br>
i'm looking for tube shapes, 6&quot; o.d. x 1&quot; wall, and <br>
4.5&quot; o.d. x 1&quot; wall<br>
<p>kenn fasanella<br><a href=mailto:kenn@research.nj.nec.com>kenn@research.nj.nec.com</a><br><a href= > </a><br>
 
Kenn,<br>Anticorodal-100 is a commercial ref for Allussuisse for the AlMgSi1 aluminum.<br>So, I thing you can get some more info in their web site or e-mailing them.<br> <p>Andrade<br><a href=mailto:jaandrade@isq.pt>jaandrade@isq.pt</a><br><a href= de Soldadura e Qualidade</a><br>
 