Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations 3DDave on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Looking for reference on max holes size for 3/4" A325

Status
Not open for further replies.

dlclarkii

Structural
Mar 29, 2005
37
Somewhere I saw it was 13/16" is the max hole size for 3/4 but I can't find the reference. Anyways that max hole size for any structural bolt is 1/16" oversized correct?
 
Replies continue below

Recommended for you

Are you steel to steel, or steel to concrete? Steel to steel I think its 1/8" bigger for oversized than standard. For steel onto concrete (anchor bolts) you can go bigger but provide washer plates as needed.
 
The max is whatever the EOR says it is. There are some guidelines, standard practices, etc., but it's ultimately up to the EOR. Why?
 
Std. bolt holes are indicated in AISC 360-10 Table J3.3 For a 3/4" Dia. A325 the std hole dia. is 13/16 (i.e. bolt diameter + 1/16") In calculations involving bolt holes an additional 1/16" is customarily added to the bolt hole dimension to account for local damage due to drilling of the hole. (I thought this was in AISC as well but I can't recall where).
 
driftLimiter said:
(I thought this was in AISC as well but I can't recall where).

AISC 360-16 Chapter B, section B4, clause 3b. The commentary states: