Does anyone know of a lab in Canada or USA that could perform some wear resistance tests on a few copper based alloys ?

Thanks
 
I use:

Lewis Research, Inc.
33712 Wescoats Road, Unit #1
Lewes, DE 19958
(302) 644-0881 • FAX (302) 644-0882
 
Zane Lockhart
Senior Metallurgist and Failure Analyst at Sherry Laboratories
Louisville, Kentucky
Sherry Laboratories
9301 Innovation Drive Suite 103
P.O. Box 569
Daleville, IN 47334-0569
Phone: 765.378.4101
Fax: 765.378.4107


Thomas J. Walz
Carbide Processors, Inc.

Good engineering starts with a Grainger Catalog.
 
NRC boucherville, Qc, Canada.

Luxeal
 
Is the wear experienced in service due in some part to erosion?
"Results" of a test method using abrasion can be very misleading.
The outfit I worked for made a bunch of material decisions doing that and some of the results were di$appointing.

regards,
Dan T
 
Tmoose, that's a good point. I think the type of testing desired would more correctly be described as "wear rate" testing, rather than "wear resistance" testing. "Wear resistance" is subjective, while "wear rate" can be quantified.
 
The main problem is finding a lab that could perform a Galling Test. Any further suggestions would be appreciated.
 
dshore, have you contacted any of the suggestions listed above yet to see if they will be able to perform your testing?
 
Bureau of Mines
at Oregon State University
Margaret Ziomek Mrosz
I saw her work on carbide a few years ago and was impressed.

FP Innovations in Canada does a lot of this but the FP stands for Forest Products so they are limited.

Thomas J. Walz
Carbide Processors, Inc.

Good engineering starts with a Grainger Catalog.
 
Which ASTM galling tests are you looking for ? I do not have very successful experience with ASTM Galling test. You may want to consider developing your own test for your own application.