Looking to coat a brown stock storage tank. If anyone has any info please let me know.
The vapor space gas is the zone we are most concerned about, there is severe corrosion.
Components measured were dimethyl sulhide and dimethyl disulphide.
Humidity 100%
The liquid components of the tank run at about 70-80 degrees celsius
With a pH of around 11
The vapor space gas is the zone we are most concerned about, there is severe corrosion.
Components measured were dimethyl sulhide and dimethyl disulphide.
Humidity 100%
The liquid components of the tank run at about 70-80 degrees celsius
With a pH of around 11