It's basically a monolithic tripod with a pedestal on top. About 45cm overall height, and the base fits within a 35cm diameter circle. The tripod legs stop about 1/3 of the way up.
Outdoor use all over the world
by occasionally angry/competitive athletes
should survive being landed on (ideally can be crushed and will spring back -- can have warping, stretch marks, etc. after)
paintable and bondable
Premium consumer grade materials are OK (the product is for high-end consumers, so some cost is acceptable. Ideally a cheap, common consumer product resin, though).
If the unit is tipped over one leg will be pointing up. From a safety standpoint this leg needs to buckle under the weight of a human body. From a customer satisfaction standpoint, it should spring back to at least usable shape (keeping the cosmetics would be a bonus) after unloading. This will be a rare event, but it will almost certainly happen.
I had a recommendation for Nylon 6/6 before the buckling requirement was added, and another recommendation for an ABS/PP blend after. Do either of these sound reasonable? Alternatives I should consider?
Thanks!!
Outdoor use all over the world
by occasionally angry/competitive athletes
should survive being landed on (ideally can be crushed and will spring back -- can have warping, stretch marks, etc. after)
paintable and bondable
Premium consumer grade materials are OK (the product is for high-end consumers, so some cost is acceptable. Ideally a cheap, common consumer product resin, though).
If the unit is tipped over one leg will be pointing up. From a safety standpoint this leg needs to buckle under the weight of a human body. From a customer satisfaction standpoint, it should spring back to at least usable shape (keeping the cosmetics would be a bonus) after unloading. This will be a rare event, but it will almost certainly happen.
I had a recommendation for Nylon 6/6 before the buckling requirement was added, and another recommendation for an ABS/PP blend after. Do either of these sound reasonable? Alternatives I should consider?
Thanks!!