Hello All,


I have a customer that is looking for a part that requires S690QL. Does anyone have a good ASTM substitute for this item? Also does anyone have a credible conversion table for all types of European to ASTM?

Any help will be greatly appreciated...
 
Replies continue below

Recommended for you

Look in your copy of Woodmans or your Stahlschluessel (Key to Steel).

= = = = = = = = = = = = = = = = = = = =
Plymouth Tube
 
Ed is referring to Woldman's Engineering Alloys.
 