I'm in the fluid power industry, but posting my question here because it has to do with Skydrol. Does anyone happen to have any information regarding the compatibility of Loctite Vibra-seal 517 with Skydrol? I've got a call in to Henkel, but who knows when I'll hear back from them. Thanks!
 
Answered my own question as it usually goes with material testing. Loctite Vibra Seal 517 is significantly softened within 2 hours by Skydrol 4. Not compatible for my application.
 