We are using a locking patch on 4-40 stainless screws. The patch is applied by the supplier and has a prevailing torque as high as 5 in-lbs. I find that rather high for a 4-40 screws. We have had some situations where we would engage a few clean threads, hit the patch and strip the threads on the end of the screw because the torque required to pierce the locking patch is too high.

Question is: what is a typical prevailing torque value for locking mechanism on 4-40 screws? I'm thinking of specifying MIN=1 in-lbs, MAX=2.5 in-lbs
 
Replies continue below

Recommended for you

It may be that the threads are galling and that causes the stripping. I've seen stainless screws without locking features go in finger tight a few turns and require milling to remove because of galling.

A short search suggests the range you have, but I'd still look at an anti-galling material for such small threads.
 