I am doing some R&D work and I need to source some rechargeable batteries with a fast response time for pulsed output current. About 1 amp.
Lithium ion seem to be best for our application however they seem to be available at 3V and over.
Must be less than 1.5V and over 1000 mAh. Cant use extra electronics to adapt 3V batteries.

Also looking into caps.

Can anyone help me source Lithium ion rechargeable below 1.5V.

Thanks in advance
 
Replies continue below

Recommended for you

Alan,

Without outside electronics, I don't think Li-Ion is the proper chemistry. The cathode voltage alone is double your 1.5V limit, so you're probably barking up the wrong tree.

Dan - Owner
Footwell%20Animation%20Tiny.gif
 
Ugly old horrible Ni-cad has very high current capabilities and is nominally about 1.25 volts (1.4 is full charge).

 
Just how fast? NiMH batteries tend to be be under 1.5V; in fact, it's usually quite annoying because some electronics will tag them as undercharged almost immediately upon use.

The standard NiMH AA battery is rated at 2400 mAh, but you could get that, or a D, and supplement with a capacitor as itsmoked suggests.

TTFN