In our caustic chlorine plant we are facing problem of liquid chlorine transferring from liquifier to storage tank. liquid chlorine is going through sniff t o hcl plant. so we have been forced to vent some chlorine to hypo. any suggestions.
arora
 
'facing problem' is not very informative. If you hope to get some help, you're going to have to be much more explicit in your system and the problems you are having.
 
Hi ! my name is mujtaba.im chemical engineer by profession and working in chloro alkali industry since for 2 years.
i think i can help u out
contact me at mujtaba_ali583@hotmail.com
or mujtaba583@yahoo.com
 
Hey,
I am also working in chlor-alkai plant. If you are more explicit abt your problem, i can help too

bye
 