Jun 17, 2009 #1 josito Petroleum Joined Oct 4, 2007 Messages 4 Location CL Please someone in the forum could explain me the differences of these coatings ?? are really coatings ??
Please someone in the forum could explain me the differences of these coatings ?? are really coatings ??
Jun 17, 2009 #2 SJones Petroleum Joined Apr 22, 2001 Messages 3,942 Location GB When talking about vessels, lining can be either of two things: a) a paint or coating system, e.g. glass flake epoxy or rubber b) a metallic sheathing intermittently attached to the internal surface A cladding can be defined as: http://events.nace.org/library/corrosion/MetalCoatings/Cladding.asp Naturally, there will be numerous other interpretations. Steve Jones Materials & Corrosion Engineer http://www.linkedin.com/pub/8/83b/b04 Upvote 0 Downvote
When talking about vessels, lining can be either of two things: a) a paint or coating system, e.g. glass flake epoxy or rubber b) a metallic sheathing intermittently attached to the internal surface A cladding can be defined as: http://events.nace.org/library/corrosion/MetalCoatings/Cladding.asp Naturally, there will be numerous other interpretations. Steve Jones Materials & Corrosion Engineer http://www.linkedin.com/pub/8/83b/b04