Is anybody aware of a reference for "standard" lightweight concrete masonry units, i.e. I am trying to get the allowable compressive strength. I am aware of Qlite and haydite block, however I am looking for a generic standard perhaps related to a building code, masonry institution, etc. Thanks
 
Replies continue below

Recommended for you

ASTM C 331
weight of less than 105 lb/ft**3
 