Someone in the shop had what appears to be a failure of his Li Ion battery in his Dell Lap-Top. A water-like liquid ran from the lap-top.

I would have blaimed the cat...but he doesn't have one :-D

Any experience with this kind of failure?

I remain,

The Old Soldering Gunslinger
 
Replies continue below

Recommended for you

Dell had a recall on some of their batteries, lately, for this reason. Check their website for info.
 